Type: Rolling Wire
Material: Steel
Flux Containing: Not Containing Flux
Slag Characteristic: None
Transport Package: Kaihong / Neutral / Custom etc...
Specification: AWS A5.17 F7A4-EH14
Samples:
US$ 5/kg 1 kg(Min.Order)
| Request Sample
Customization:
Gold Member Since 2022

Suppliers with verified business licenses

Rating: 5.0/5
Trading Company

Basic Info.

Model NO.
HFX-EH14
Trademark
WELDBST
Origin
P. R. C.
HS Code
72173010
Production Capacity
50000mt/Year

Product Description

       HFX-EH14 is a submerged arc welding wire of coppersurfaced carbon structural steel, Be used together with fused flux KJ105. KJ105 is fluorine-alkalil and high alkali & low hydrogen agglomerated flux, It appears a ball granule of gray color about 10~60 mesh in size. They are used together, slag is easy and high-performance to anti-pores and the welds has good crak resistance.

       Model No.: HFX-EH14
       Flux contanining: not containing flux
       Diameter: 1.6mm, 2.0mm, 2.4mm, 3.2mm, 4.0mm
       Type: Rolling wire
       Net weight:  20 kg per spool, 25/50/250 kgs per roll
       Export Markets: Gloal


      Application:
       HFX-EH14 coppersurfaced submerged arc welding wire used together with KJ105 fused flux, Using to submerged arc auto welding of low alloy steel. For example: pressure vessel nuclear power, above 40°C low temperature pressure vessel etc. metal welding of same strength class low alloy steel.


Chemical composition of wires (%)
  C Mn Si S P Cr Ni Cu
Welding wires 0.076 1.58 0.052 0.011 0.013 0.018 0.015 0.040
Deposited metals 0.065 1.25 0.350 0.009 0.015 0.010 0.034 0.044

Typical mechanical properties of deposited metal
  Tensile Strength
Rm(Mpa)
Yield Strength
REl(Mpa)
Elongation
(%)
AKV Impact value
(J)(-20°C)
Standard values 480~650 ≥400 ≥22 ≥27
Sample values 510 430 28 120

NOTICE:
        1. Dry the flux at 350~400°C for 2 hours before, completely remove rust,oil and dirt from the groove surface prior to welding.
        2. Before welding, rust, water and impurities are to be removed from the welded surfaces of workplaces.
Submerged Arc Welding Wire Eh14 H10mn2

Submerged Arc Welding Wire Eh14 H10mn2Our services
1. Free sample is available
2. OEM service is available
3. High quality and professional service.
4. Much more competitive price.
5. On-time delivery

FAQ
1. Can you provide free sample for quality testing?
    -Yes, we can provide few quantity on free base.
2.  Do you accept small order ?
    -Yes.
3.  Do you accept OEM ?
    - Yes, we accept OEM packing on FCL base.
4.  Do you accept mix items in one container ?
   - Yes.
5.  Do you have inspection procedures for product?
   - Yes, we have Mill Test Report with each shipment

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now

You Might Also Like

Gold Member Since 2022

Suppliers with verified business licenses

Rating: 5.0/5
Trading Company
Registered Capital
100000 RMB
Plant Area
<100 square meters